Suspension thermal sprayed nanocomposite WC-Co coatings: Nano-indentation assessment


10th International Conference on Emerging Materials and Nanotechnology

July 27-29, 2017 Vancouver, Canada

Matheus (Theo) F A Goosen, Omar Ali, Rehan Ahmed, Nadimul H Faisal, Nayef M Al-Anazi and Youssef O Elakwah

Alfaisal University, KSA
Heriot-Watt University, UK

ScientificTracks Abstracts: Res. Rev. J Mat. Sci

DOI: 10.4172/2321-6212-C1-002

Abstract

Statement of the Problem: Nanoindentation of WC-12Co thermal spray coatings has been used to evaluate the elastic modulus and hardness of coating on the polished surface of the coatings. While there has been much progress overall, limited research has been reported on the deposition and evaluation of WC-cermet coatings. The aim of this study was to evaluate the microstructural and nanohardness characteristics of tungsten carbide-cobalt (WC-Co) cermet coatings deposited by liquid suspension spraying. Methodology: Commercially available WC-Co coating powder was milled and water based suspension was produced as feedstock for the thermal spray coating process. Microstructural evaluations of WC-Co cermet coatings included XRD (X-Ray Diffraction) and SEM (Scanning Electron Microscopy). Post spraying nanomechanical evaluations were conducted using a Berkovich nanoindenter. Findings: Results indicated relatively higher modulus but lower hardness of suspension coatings. The load displacement curves during nanoindentation were characteristic of the complex coating microstructure showing signs of microcracking and pileup. The load displacement (P-h) curves along with the SEM images of indents for S-HVOF (suspension high velocity oxyfuel) coating illustrated evidence of sink-in and pile-up of material around the indent contact residual impression during the nanoindentation process. There was some indication of microcracking during indentation as well. Conclusions: A comparison of S-HVOF and conventional HVOF coatings points toward phase transformations occurring in the suspension spraying which led to nanocrystalline or amorphous phases. The elastic modulus of S-HVOF coatings was on average higher than the conventional HVOF coating. The load displacement curves show features which are consistent with the complex coating microstructure with evidence of micro-cracking and pile-up.

Biography

Mattheus (Theo) F A Goosen has played key roles in the development of new start up academic institutions. For the past nine years he has held the position of founding Associate Vice President for Research & Graduate Studies at Alfaisal University a private start-up non-profit institution in Riyadh, Saudi Arabia. He has obtained a Doctoral degree in Chemical & Biomedical Engineering from University of Toronto, Canada in 1981. He has more than 180 publications to his credit including over 133 refereed journal papers, 45 conference papers, 10 edited books and 10 patents. His H-index is over 47 and has over 8000 citations on Google Scholar. On Scopus he has 133 publications with over 4000 citations. His research interests are in the areas of renewable energy, desalination, sustainable development, membrane separations, spray coating technology and biomaterials.

https://pmasites.com/https://casinositeleriniz.com/https://fbhesq.com/
Spanishenglish.com spanishenglish.com helps to translate Spanish to English and English to Spanish for free.
Turkceingilizce.gen.tr kullanarak 100'den fazla dil ciftinde hemen ceviriler yapabilirsiniz.ingilizce turkce ceviri turkceingilizce.gen.tr

freetranslations.org/english-to-spanish-translation.html helps to translate English to Spanish to English for free.
ingilizceturkce.gen.tr ingilizce turkce ceviri, turkce ingilizce ceviri, ingilizce turkce cumle ceviri, ingililizceyi turkceye ceviri ve turkceyi ingilizceye ceviri gibi tum dillerde dogru ceviri hizmetleri sunuyor.
Turkceingilizce.gen.tr kullanarak 100'den fazla dil ciftinde hemen ceviriler yapabilirsiniz.ingilizce turkce ceviri turkceingilizce.gen.tr

https://babesoflondon.com/